5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet

Product Details
Customization: Available
Application: Transportation Tools, Auto Body Sheet
Certification: ISO9001, JIS, GB, EN
Still deciding? Get samples of US$ 0/Piece
Request Sample
Manufacturer/Factory, Trading Company
Diamond Member Since 2018

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Registered Capital
3000000 RMB
Plant Area
101~500 square meters
  • 5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet
  • 5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet
  • 5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet
  • 5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet
  • 5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet
Find Similar Products
  • Overview
  • Detailed Photos
Overview

Basic Info.

Model NO.
5182/5754
Grade
5000 Series
Temper
O - H112
Surface Treatment
Mill Finish
Alloy
Alloy
Transport Package
Export Standard Wooden Case
Specification
According to Customer Requirement
Trademark
Chalco Aluminum
Origin
Henan China
HS Code
7606125900
Production Capacity
20000mt/Month

Product Description

5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet

The production of car body, especially the production of all kinds of manned vehicle body, is the quintessence of the automobile industry. The body building almost takes up 30% of the total investment of the automobile manufacturing company. The quality of the body is 30% of the total mass, and the reduction of its quality plays a vital role in reducing the quality of the vehicle.

Aluminum sheet for manned vehicle

The brand and chemical composition of the ABS plate aluminum alloy of the car body are shown in the following table. With 2 series, 5 series and 6 series in the body can, 7 series alloys, in addition to 5 series alloy, three other alloys are heat treatment can enhance the strength in their painting baking (170--200 C, 20--30min) has been further improved, for the manufacture of high light and high rigid plate, the strength of 6*** alloy although low, but the plastic forming performance, used in the manufacture of complex shaped plate. 6009 and 6010, the strength of the body plate alloy after T4 treatment is lower than that of 5182-O and 2036-T4 alloy, but the plasticity is quite high. After molding, the artificial aging can achieve higher strength in the process of spraying and baking. These two alloys can be used to make both inner and outer panels separately, or 6009 alloy to make inner wall panels, and two with 6010 alloy to make outer wall panels.

The thickness of the sheet metal parts for the car body of a manned vehicle is 0.9--1.3mm, and about 19 panels per car. Body parts of large size and complex shape, mainly through punching and bulging two composite molding production, and the latter mainly. The joint of the sheet metal parts is welded or bonded, and it is also linked to the fastener.

 
ABS Aluminum Sheet Chemical Compostion
Alloy Si Fe Cu Mn Mg Cr Zn Ti Others Aluminum Min.
Each Total
5182 0.20 0.35 0.15 0.20-0.50 4.0--5.0 0.10 0.25 0.10 0.05 0.15 Remainder
5754 0.40 0.40 0.10 0.50 2.6--3.6 0.30 0.20 0.15 0.05 0.15 Remainder
6016 1.0--1.5 0.50 0.20 0.20 0.25--0.6 0.10 0.20 0.15 0.05 0.15 Remainder
6014 0.30-0.60 0.35 0.25 0.05--0.20 0.40--0.8 0.20 0.10 0.10 0.05 0.15 Remainder
 
ABS Aluminum Sheet Physical Property( thickness 0.9mm--1.3mm)
Alloy Temper 90º Bending radius cupping value/mm N Value R Value Tension Strength Rm/N.mm¯² Yield Strength Rp0.2/N.mm¯² Elongation As/%
5182 - O 1/2t   0.33 0.80 28.1 13.3 26
5754 - O 1/2t   0.31 0.67 215 108 53
6016 - T4 1/2t 10 0.26 0.75 24.0 13.0 26
6014 - T4 1/2t   0.26 0.65 17.9 13.0 23
6111 - T4 1/2t 8.4     29.6 16.2 26

The aluminum sheet of the ABS body also needs to have the performance:
A. Good formability.

Forming the body and cover of the metal plate is moved over from the aviation industry, the Aluminum Alloy  automotive body sheet forming should have good formability, which has low yield ratio and high forming limit (FLC forming, limit curve), with very high space forming stress deformation in stamping different.




B. Surface roughness

Aluminum Alloy must have good ductility and flanging forming after surface color consistent performance of the sheet metal forming surface does not appear in Luoping line (roping line), namely the slip line. It is due to uneven grain or uneven distribution of inclusions, resulting in uneven surface deformation of the sheet, so that the surface is inconsistent after the paint.

B. Good weldability.

Good welding performance meets the requirements of continuous welding process for automobile construction after forming. The plate should have anti ageing stability, to ensure that the board before the factory to the stamping production without limitation, prevent the stamping of the yield point of the material increased, induced by Lu De with (Lude 's zone) surface caused by uneven deformation and wrinkling, thus affecting the surface quality of automobile outer panels.

D. Excellent baking hardening

Lightweight automobile also requires plate with high bake hardening, the yield strength of plate after stamping deformation and paint baking increased, so as to ensure the stamping sheet metal paint after high dent resistance, compatibility Aluminum Alloy plate paint baking process and the steel stampings especially baking process the.

5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet




Specification of aluminum automotive body sheet:

Alloy: 5182, 5754, 6016, 6014, 6111
Temper: T4, O
Surface treatment: EDT, Prelubrication, Primer coated
Strip/sheet width: 1000-2300mm
Strip/sheet gauge: 0.6--3.2mm
Capacity: 100 000 tonne/ year

Car body aluminum sheet pretreatment line


Surface Topography for car body sheet

Established surface topography is EDT(electric discharge texturing), transferred to the strip surface from texturized rolls during the last rolling pass.
 
5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet


Advantage of EDT topography
1) Isotropic, no directional influence on forming behaviour
2) Lubrication pockets lead to build up of hydrostatic pressure
Low and regular friction coefficient;
Better formability than with Mill finish surface
Less pick-up of work piece material on the tool surface
Regular press parameters
3) Stochastic surface structure
Good lacquer appearance

Chemical and electrochemical pretreatments
Different types of pretreatments can be applied on the strip surface--depending on the costomer requirements:
1) Degreasing
2) Pickling
3) Conversion treatments
Ti- or Ti/Zr-fluoride based agents, without or which polymer addition, mainly for hem flange bonding,
As pretreatment for primer or prelacquer application.
Prelubrication
Advantages of dry lubrication sheet
1) surface protection during transport and storage
2) Automatic destacking of panels in the press shop
3) No oiling operation
4) No operators at line entry to remove interleave paper
5) Improved formability compared to drawing oil
6) Constant friction conditions during pressing
7) Increased stamping rate
8) Less problems with surface contamination
9) Compatible with mechanical joining and bonding
10) Removable with mild alkaline degreasing agents
11) E-coat compatible products are available

Combination of conversion+lubrication+ PX treatment on the Al strip= combination of the advantages
5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet


Advantages of primer coated sheet
1) surface protection, during transport and handling
2) Improved formability(lubrication still required)
3) Protection against corrosion
4) Good basis for bonding
5) Good basis for lacquering, less influence of the Zn-phosphating conditions
6) Surface appearance of lacquered Al parts compatible with that of steel parts.

Primer coated strip--benefit for car producer
1) easier processing of aluminum sheet on equipment optimized for steel
2) Suitable for use in mixed metal constructions
3) Grinding of the formed panels, reduction of the corrosion resistance
4) Not weldable, bonding and mechanical joining
5) Recyclability, less value of process scrap
Detailed Photos

 

5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet5182/5754 O Aluminum Automotive Automobile Vehicle Car Body Sheet

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier
Product Groups
More