4343/3003 Aluminum Alloy Brazing Strip Coil

Product Details
Customization: Available
Application: Air Cooling Fin
Certification: ISO9001, ASTM, GB
Still deciding? Get samples of US$ 0/Piece
Request Sample
Manufacturer/Factory, Trading Company
Diamond Member Since 2018

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Registered Capital
3000000 RMB
Plant Area
101~500 square meters
  • 4343/3003 Aluminum Alloy Brazing Strip Coil
  • 4343/3003 Aluminum Alloy Brazing Strip Coil
  • 4343/3003 Aluminum Alloy Brazing Strip Coil
  • 4343/3003 Aluminum Alloy Brazing Strip Coil
  • 4343/3003 Aluminum Alloy Brazing Strip Coil
  • 4343/3003 Aluminum Alloy Brazing Strip Coil
Find Similar Products

Basic Info.

Model NO.
4343/3003
Technique
Hot Rolled/Cast Rolled
Grade
3000 Series 4000 Series
Temper
O/H14
Surface Treatment
Mill Finish
Alloy
Alloy
Transport Package
Export Standard Wooden Pallet
Specification
According to Customer Requirement
Trademark
Chalco Aluminum
Origin
Henan China
HS Code
7606119000
Production Capacity
10000mt/Month

Product Description

4343/3003 aluminum strip coil for Air Cooling Fin

3003 aluminum strip coil foil for Charge Air cooler

Of all the methods available for metal joining, brazing may be the most versatile. Brazed joints have great tensile strength - they are often stronger than the two metals being bonded together. Brazed joints repel gas and liquid, withstand vibration and shock and are unaffected by normal changes in temperature. Because the metals being joined are not themselves melted, they are not warped or otherwise distorted and retain their original metallurgical characteristics.

*Various kinds of specification for fin

*Excellent collapse resistance during brazing

 
Performance index of charge air cooler fin material
Alloy Temper
 
Thickness
(mm)

 
Tolerance
(mm)

 
Clad rate(%)
 
Mechanical property
Tensile Strength
(MPa)
Yield
Strength
(MPa)
Elongation
Min.(%)

 
4343/3003/4343 H14 0.1~0.12 ±0.005 8~12 150~200 ≥120 1
4345/3003/4345 H14 0.1~0.12 ±0.005 8~12 150~200 ≥120 1
3003 H14 0.08~0.12 ±0.005 None 150~200 ≥120 1

*4343 can be replaced by 4045/4047/4104/4004etc, according to customer's requirement.

*Alloy,specification and mechanical property can be customized according to different requirement.

 

Method of brazing:
The step by step procedure for brazing is as follows:
1.The metal parts which are to be brazed must be thoroughly cleaned.
2.The flux must be applied to the surface.  
3.The parts are to be clamped in the required position.
4. The flux ha to be applied on the surfaces.  
5.The job has to be heated using the blow torch or the furnace etc.
6. The molten spelter has to be allowed to flow by capillary action into the joint.  
7.The job has to be allowed to cool slowly.

*Perfect brazing feature, fit for any furnace    

*Good consistency for any fin mill

*Excellent collapse resistance during brazing


 
Performance index of air cooling fin materials
Alloy Thickness(mm) Tolerance(mm) Clad rate (%)
4343/3003 0.25-8.3 ±0.007 13~17
4343/SA-7/4343 0.25-8.3 ±0.007 13~17

*OD: 1800max;
*Width tolerance:±0.02mm; 
*Alloy,specification and mechanical property can be customized according to different requirement.


 
4343/3003 Aluminum Alloy Brazing Strip Coil4343/3003 Aluminum Alloy Brazing Strip Coil4343/3003 Aluminum Alloy Brazing Strip Coil4343/3003 Aluminum Alloy Brazing Strip Coil4343/3003 Aluminum Alloy Brazing Strip Coil4343/3003 Aluminum Alloy Brazing Strip Coil


 

Send your message to this supplier